Transmission oil RENA TSZp-8


Transmission oil RENA TSZp-8
Extreme winter transmission oil TSZp-8. Guarantees flawless fluidity and gearbox protection at temperatures down to -50°C.
Operating special equipment in the Far North or at abnormally low temperatures imposes the strictest requirements on lubricants. RENA TSZp-8 is a unique winter transmission oil that guarantees trouble-free operation of gearboxes and axles in frosts down to -50°C. Its ultra-fluid formula prevents the lubricant from freezing, relieving the load from the starter and ensuring instant oil delivery to friction units. The product effectively neutralizes moisture formed from temperature changes. Contact our specialist to conclude a supply contract.
Specialized SAE 75W-80 class oil. Kinematic viscosity at 100°C is 8.0 mm²/s, viscosity index — 140. Extreme pour point reaches -50°C. Weld load 3280 N. Meets API GL-3 classification.
Technical Specifications
| Parameter | Value | Test Method |
|---|---|---|
| Density at 20 °C | 0.900 g/cm³ | ASTM D 4052 |
| Kinematic viscosity at 100 °C | 8.0 mm²/s | ASTM D 445 |
| Viscosity index | 140 - | ASTM D 2270 |
| Flash point (open cup) | 170 °C | ASTM D 92 |
| Pour point | -50 °C | ASTM D 97 |
| Mechanical impurities content | 0.025 % | п. 7.3 |
| Water content | Сліди % | ASTM D 95 |
| Sulfated ash content | - % | ASTM D 874 |
| Sulfur content | <0.7 % | ASTM D 6481 |
| Phosphorus content | ≥0.08 % | ASTM D 6481 |
| Total acid number (TAN) | - mg KOH/g | ASTM D 664 |
| Color | 4.0 - | ASTM D 1500 |
| Copper strip corrosion (120 °C, 3 h) | Витримує - | ASTM D 130 |
| Foaming at 24 °C / stability | 350/0 ml/ml | ASTM D 892 |
| Foaming at 93.5 °C / stability | 150/0 ml/ml | ASTM D 892 |
| Weld load (4-ball tester) | 2764 N | ASTM D 2783 |
Density at 20 °C
Value
0.900 g/cm³
Test Method
ASTM D 4052
Kinematic viscosity at 100 °C
Value
8.0 mm²/s
Test Method
ASTM D 445
Viscosity index
Value
140 -
Test Method
ASTM D 2270
Flash point (open cup)
Value
170 °C
Test Method
ASTM D 92
Pour point
Value
-50 °C
Test Method
ASTM D 97
Mechanical impurities content
Value
0.025 %
Test Method
п. 7.3
Water content
Value
Сліди %
Test Method
ASTM D 95
Sulfated ash content
Value
- %
Test Method
ASTM D 874
Sulfur content
Value
<0.7 %
Test Method
ASTM D 6481
Phosphorus content
Value
≥0.08 %
Test Method
ASTM D 6481
Total acid number (TAN)
Value
- mg KOH/g
Test Method
ASTM D 664
Color
Value
4.0 -
Test Method
ASTM D 1500
Copper strip corrosion (120 °C, 3 h)
Value
Витримує -
Test Method
ASTM D 130
Foaming at 24 °C / stability
Value
350/0 ml/ml
Test Method
ASTM D 892
Foaming at 93.5 °C / stability
Value
150/0 ml/ml
Test Method
ASTM D 892
Weld load (4-ball tester)
Value
2764 N
Test Method
ASTM D 2783
Laboratory Services
Recommended Laboratory Analyses
Maximize your equipment lifespan with our state-of-the-art diagnostic services tailored for this specific product category.
| Analysis Title | Category | Price | Details |
|---|---|---|---|
| Viscosity Index (VI) | Motor oils | 1500 | Details › |
| Brookfield Dynamic Viscosity | Gear oils | 1800 | Details › |
| Flash Point by Cleveland Open Cup | Industrial oils | 850 | Details › |